  1. Chemistry
  2. The carbon question
  3. Properties that matter in use
  4. Where each grade goes
  5. A note on purity grades
  6. Frequently asked questions

Ni200 and Ni201 are the same metal at different carbon levels. Everything else — corrosion behaviour, thermal conductivity, electrical resistivity — is close enough that the choice usually comes down to one question: how hot, and how much carbon can it afford to pick up? Both grades are drawn in our own factory, so we can hold the carbon window, not just quote it.

Chemistry

Ni200 (N02200)Ni201 (N02201)
Nickel≥ 99.0%≥ 99.0%
Carbon≤ 0.15%≤ 0.02%
Iron≤ 0.40%≤ 0.40%
Sulphur≤ 0.01%≤ 0.01%
Typical resistivity0.0684 µΩ·m0.0684 µΩ·m

The carbon question

Carbon in nickel is harmless below roughly 315 °C. Above that, carbon from graphite-bearing lubricants, packing or atmospheres diffuses into the metal and precipitates as graphite at grain boundaries — the material slowly turns brittle from the inside. Ni201 exists for exactly this regime: with carbon capped at 0.02%, the embrittlement mechanism has nothing to work with.

Properties that matter in use

  • Magnetic below 358 °C (the Curie point), non-magnetic above it — worth remembering if a design assumes constant permeability.
  • Excellent caustic resistance: nickel is the default metal for sodium and potassium hydroxide.
  • Good thermal and electrical conductivity for a nickel alloy — hence its use as a current path in battery tabs.
  • Welds cleanly with ERNi-1 filler; solderability is acceptable after surface activation.

Where each grade goes

  • Ni200: general vacuum hardware, electronic leads, plating racks, caustic handling below 315 °C.
  • Ni201: anything hotter, parts in contact with graphite, caustic evaporators, and battery tab strip where process heat is applied.

A note on purity grades

Ni200 and Ni201 are commercial grades. Where the application needs controlled trace elements — evaporation sources, sputtering targets, analytical ware — the right product is 4N (99.9%) or 5N (99.99%) nickel, quoted with GDMS or ICP-MS trace analysis rather than a standard MTR alone.

Key takeaways

  • The difference is carbon, and it decides the temperature limit. Ni201 keeps carbon at or below 0.02%, which prevents graphitisation above roughly 315 °C.
  • Ni200 is the general-purpose grade. Below 315 °C, Ni200 performs identically at lower cost and better availability.
  • Both are commercially pure, not alloyed. The 99.6% and 99.0% figures describe nickel content, not a performance ranking.
  • Purity grades are a separate axis. 4N (99.9%) material for electronics is specified by oxygen and trace elements, not by the Ni200/Ni201 designation.

Frequently asked questions

When must I use Ni201 instead of Ni200?

Above roughly 315 °C. Ni200 contains up to 0.15% carbon, and in the 315–600 °C range that carbon can migrate to grain boundaries and form graphite, embrittling the wire. Ni201 holds carbon at 0.02% maximum and avoids the mechanism.

Are Ni200 and Ni201 interchangeable at room temperature?

For most mechanical and electrical purposes, yes. Mechanical properties, resistivity and corrosion behaviour are effectively the same. The difference appears at elevated temperature and in welding, where the lower carbon of Ni201 also reduces sensitisation risk.

What does 4N purity mean, and do I need it?

4N means 99.99% nickel. It is specified for vacuum devices, electron tubes and analytical instruments where trace elements affect emission or outgassing. If your part is a battery tab or a caustic-service component, standard Ni200 or Ni201 is sufficient and less expensive.

Is pure nickel wire magnetic?

Yes, at room temperature. Nickel is ferromagnetic below its Curie point of about 358 °C. If your application requires non-magnetic behaviour, this grade is the wrong choice.

Can Ni200 be used in sulphur-bearing atmospheres?

Not above roughly 315 °C. Nickel reacts with sulphur compounds to form nickel sulphide at grain boundaries, causing rapid embrittlement. This is true of both grades and is a chemistry limit, not a carbon one.

D GO TOP Technical Team

Process Engineering · Wire Drawing & Heat Treatment

Our engineers support grade selection, element sizing and tolerance review for nickel, nickel-chromium, FeCrAl and superalloy wire. More about our technical team.

Next step

Send three numbers, get an answer

Diameter or cross-section, working temperature, and required power or resistance. We reply within 24 hours with the grade that fits, and with where the margin sits.

WhatsApp UsContact Us