A sealing bar that runs two degrees hot scorches the film; two degrees cold gives a weak seal. Repeatable resistance is the whole game.
The three requirements that decide whether the wire works here.
Element wattage has to stay inside the tolerance your controller and process can absorb, lot after lot.
Oxide scale growth, sag and grain growth set the replacement interval — not the data sheet maximum.
Traceability from melt to spool, with the certificate formats your quality system expects.
Starting points — the final choice follows the atmosphere, cycle and geometry.
| Application | Grade | Typical size | Why |
|---|---|---|---|
| Sealing band | Ni80Cr20 flat | 0.2 × 1.5 mm | Uniform temperature along the bar |
| Impulse sealer | Ni80Cr20 | 0.3–0.6 mm | Fast thermal response |
| Hot-cut knife | Ni80Cr20 | 0.5–1.0 mm | Edge retention at 400 °C |
| Thermocouple lead | Constantan + Ni80Cr20 (Type E) or Cu (Type T) | 0.2–0.5 mm | Constantan is the negative leg of both types |
Yes — send a sample or the resistance per metre and we will match within ±3%, so the machine does not need re-tuning after a wire change.
Almost always uneven clamping pressure or a cold end where the terminal is. Check the terminal joint first; if the band itself is oxidising unevenly, the surface load is too high for the cycle time.
We supply flat wire cut to length and, for volume orders, pre-formed with welded terminals to your drawing.
Service temperature, atmosphere, cycle time and joint design — with those four numbers we can recommend a grade and size with the life you need.