Commercially pure nickel drawn to wire, rolled to strip and forged to bar — for vacuum components, battery tabs, electronic leads and caustic chemical service. Ni200 for general work, Ni201 where carbon pickup cannot be tolerated.
Each series is a separate page with grades, tolerances, forms and packing.
Drawn wire from 0.05 to 5.0 mm, bright annealed, P5/P4 tolerance. The default choice for vacuum hardware and electronic leads.
4N nickel for electroplating baskets, evaporation filaments and analytical equipment where trace elements matter.
Rolled strip 0.05–2.0 mm for battery tabs, spot-welding tabs and connector stampings, supplied in traverse-wound coils.
Forged and rolled bar, rod and plate for flanges, electrodes, anodes and machined components.
Indicative data — the order confirmation carries the binding specification.
| Grade | UNS / GB | Key data | Typical use |
|---|---|---|---|
| Ni200 | N02200 / N6 | Ni ≥ 99.0%, C ≤ 0.15% | Caustic handling, vacuum parts, electronic leads |
| Ni201 | N02201 / N4 | Ni ≥ 99.0%, C ≤ 0.02% | Above 315 °C, where carbon pickup would embrittle |
| Nickel 99.9% | 4N | Ni ≥ 99.9%, low S/P/Fe | Plating baskets, evaporation sources, lab ware |
| Nickel 99.99% | 5N (on request) | Ni ≥ 99.99% | Sputtering targets, semiconductor components |
Three questions that decide the grade before price is discussed.
The only real difference is carbon: 0.15% max in Ni200, 0.02% max in Ni201. Below roughly 315 °C either works. Above that, graphite-containing lubricants and carbon-bearing atmospheres will push carbon into Ni200 and graphitise the grain boundaries — specify Ni201.
Anything wound, woven or bent repeatedly wants drawn round wire. Battery tabs and connector stampings want flat strip, because the weld nugget and current path are better controlled on a flat section.
Standard bright annealed wire carries a light oxide-free surface. For vacuum and electronic use specify ultrasonic degreasing plus a brightness check; for plating baskets the surface must be free of drawing lubricant or the bath contaminates.
Coil and spool numbers linked to the melt.
Chemistry, mechanicals, dimensions.
Against the agreed standard.
SGS, BV or TÜV on request.
Carbon content: Ni200 allows up to 0.15%, Ni201 only 0.02%. Ni201 is specified above about 315 °C and wherever the part sees carbon-bearing lubricants or atmospheres, because carbon embrittles nickel at grain boundaries.
Yes, down to 0.05 mm in Ni200 and Ni201 on spools from 0.5 kg. Below 0.08 mm we recommend a draw-and-anneal route with intermediate cleaning and quote a minimum order of 3 kg.
Every shipment carries an EN 10204 3.1 mill test report with chemistry, mechanical properties and the coil or spool number, plus a certificate of conformity. Third-party inspection such as SGS or BV can be arranged on request.
Nickel-to-aluminium ultrasonic welding is done routinely for battery tabs; nickel-to-nickel spot welding is easier still. Tell us the tab thickness so we can hold the strip tolerance and surface finish that the weld schedule expects.
Send the grade, size, quantity and service conditions. An engineer replies within 24 hours with a quotation and, if useful, a grade recommendation.