Two families, one purpose: predictable resistance at temperature. FeCrAl for the highest element temperatures and lowest cost per kilowatt-hour; nichrome for strength, ductility and the widest availability.
Each series is a separate page with grades, tolerances, forms and packing.
0Cr25Al5, 0Cr21Al6, 0Cr21Al6Nb and 0Cr27Al7Mo2 for furnace elements, radiant tubes and ceramic-supported heaters.
Ni80Cr20, Ni60Cr15 and Ni35Cr20 for appliance heating, resistance units and sheathed elements.
Constantan (CuNi44) and Manganin (CuMn12Ni) with a low temperature coefficient for shunts and resistors.
Flat strip for ribbon elements and stranded or braided conductors for flexible leads and high-current joints.
Heavy-gauge FeCrAl for 1,300 °C service in industrial furnaces, with the creep and sag data your element design needs.
Indicative data — the order confirmation carries the binding specification.
| Grade | UNS / GB | Key data | Typical use |
|---|---|---|---|
| 0Cr25Al5 | FeCrAl | 1.42 µΩ·m · 1,300 °C | General furnace elements, lowest cost per kg |
| 0Cr21Al6 | FeCrAl | 1.23 µΩ·m · 1,250 °C | Appliance and oven elements |
| 0Cr21Al6Nb | FeCrAl + Nb | 1.45 µΩ·m · 1,350 °C | Better hot strength, less sag in long elements |
| 0Cr27Al7Mo2 | FeCrAl + Mo | 1.53 µΩ·m · 1,400 °C | Highest temperature, ceramic fibre modules |
| Ni80Cr20 | Nichrome | 1.09 ±0.05 µΩ·m · 1,200 °C | General purpose elements, best ductility |
| Ni60Cr15 | Nichrome | 1.12 µΩ·m · 1,150 °C | Cost-driven elements with good oxidation resistance |
| Ni35Cr20 | Ni-Cr-Fe | 1.04 µΩ·m · 1,100 °C | Domestic appliances, lower nickel content |
| Ni70Cr30 | Nichrome | 1.18 µΩ·m · 1,200 °C | Higher resistivity nichrome for compact elements and long life |
| Constantan CuNi44 | Cu-Ni | 0.49 µΩ·m · low TCR | Shunts, resistors, thermocouple legs |
| Manganin CuMn12Ni | Cu-Mn-Ni | 0.43 µΩ·m · ±10 ppm/K | Precision resistors, calibration standards |
Three questions that decide the grade before price is discussed.
FeCrAl wins on temperature (up to 1,400 °C), resistivity and price. Nichrome wins on ductility after service, on strength at temperature, and on behaviour in reducing or vacuum atmospheres where the alumina scale of FeCrAl cannot form properly. Above 1,200 °C, there is no nichrome option.
Resistance per metre fixes the wire length for a given wattage. A higher-resistivity grade means a shorter, thicker wire — often cheaper and stronger. Send us power, voltage and element geometry and we will size it with you.
Every element grows a scale. FeCrAl grows alumina, which is protective but brittle when cold; nichrome grows chromia, which spalls on thermal cycling. Winding, support spacing and start-up procedure all affect service life more than grade alone.
Coil and spool numbers linked to the melt.
Chemistry, mechanicals, dimensions.
Against the agreed standard.
SGS, BV or TÜV on request.
Aluminium in the alloy forms a protective alumina scale. After the first firing, the wire loses most of its room-temperature ductility, so elements must be designed not to need re-bending after installation. Grain growth at high temperature adds to the effect.
Yes. We hold resistivity within ±3% on request and can certify resistance per metre or per kilogram. For element production this is usually more useful than a diameter tolerance alone.
0Cr25Al5 to 1,300 °C, 0Cr27Al7Mo2 to 1,400 °C, Ni80Cr20 to 1,200 °C, Ni60Cr15 to 1,150 °C. In reducing atmospheres or vacuum these limits drop sharply — tell us the atmosphere, it changes the answer.
Yes: flat strip from 0.1 × 0.8 mm, and stranded or braided constructions for flexible leads. Stranded conductors are quoted with the equivalent cross-section and resistance per metre.
Send the grade, size, quantity and service conditions. An engineer replies within 24 hours with a quotation and, if useful, a grade recommendation.