Skip to content
Home / Products / Nickel-Based Alloys
Product category 02

Nickel-Based Alloys — Manufactured in Our Factory

Superalloys, corrosion-resistant alloys, iron-nickel superalloys and controlled-expansion grades — drawn to wire for furnace fixtures, chemical plant, heat exchangers, fasteners and glass-to-metal seals.

5product series
0.10–8.0 mmdrawn wire
1,100 °Cservice ceiling
20+grades stocked

Products in this category

Each series is a separate page with grades, tolerances, forms and packing.

Grades and typical applications

Indicative data — the order confirmation carries the binding specification.

GradeUNS / GBKey dataTypical use
Inconel 600N0660072Ni-15Cr-8FeFurnace fixtures, thermocouple sheaths, caustic service
Inconel 601N0660160Ni-23Cr-1.4AlHigh-temperature oxidation, kiln parts
Inconel 625N0662558Ni-21Cr-9Mo-3.6NbMarine, chemical, seawater, bellows
Inconel 718N07718Ni-Cr-Fe-Nb-Mo, age hardenedFasteners, springs, cryogenic hardware
Inconel X-750N07750Ni-Cr-Fe-Ti-Al, age hardenedSprings and seals to 700 °C (continuous)
Monel 400N0440063Ni-28CuHydrofluoric acid, seawater, salt water
Monel K500N05500Ni-Cu-Al-Ti, age hardenedPump shafts, valve trim, marine fasteners
Hastelloy C-276N1027657Ni-16Mo-15Cr-4WWet chlorine, mixed acids, flue gas desulphurisation
Hastelloy C-22N0602256Ni-22Cr-13Mo-3WOxidising + reducing media, pulp bleach
Hastelloy B-2N1066565Ni-28MoHydrochloric acid, sulphuric acid
Incoloy 800 / 800HN08800 / N0881032Ni-21Cr-FeReformer and cracking furnace tubing
Incoloy 825N0882542Ni-21Cr-3Mo-2CuSulphuric and phosphoric acid, seawater cooling
Incoloy 925N0992542Ni-21Cr-3Mo-2Cu-Ti-Al, age hardenedOil & gas downhole, sour service
GH4169GH4169 = 718GB equivalent of Inconel 718Domestic substitution, aerospace fasteners
GH3030≈ Nimonic 75 / N06075Ni-20Cr solid solutionFurnace parts and fixtures in the 1,000 °C class
GH3128no Western equivalentNi-Cr-W-Mo solid solutionGas-turbine combustor liners, nozzle guides
GH2132A-286 / UNS S66286Fe-Ni-Cr age hardenedBolting and discs in 650 °C service
4J29 / 4J36Kovar / InvarFe-29Ni-17Co / Fe-36NiGlass-to-metal seals, precision instruments
1J50 / 1J79Fe-Ni soft magneticFe-49Ni / 79Ni-4Mo permalloyTransformers, magnetic shielding, relays

How to choose

Three questions that decide the grade before price is discussed.

Start from the environment, not the grade name.

Oxidising or reducing? What temperature? Chlorides present? Inconel 600 handles oxidising atmospheres to 1,100 °C but is attacked by hydrochloric acid; Hastelloy B-2 is built for hydrochloric acid but not for oxidising media. Getting this order wrong is the most expensive mistake in alloy selection.

Ask what the wire is doing mechanically.

A heating-element support that only holds weight can be 600. A spring that cycles 106 times at 600 °C wants X-750 or 718 in the aged condition. Tell us the stress, and we will quote the temper with the wire.

Chinese GH grades are not drop-in equivalents.

GH4169 matches Inconel 718 closely, but GH3030 and GH3128 have no exact ASTM counterpart. If your drawing calls for a GH grade, send the composition with the order rather than relying on the name.

Quality documents with every lot

01

Heat traceability

Coil and spool numbers linked to the melt.

02

EN 10204 3.1

Chemistry, mechanicals, dimensions.

03

Certificate of conformity

Against the agreed standard.

04

Third-party inspection

SGS, BV or TÜV on request.

Questions buyers ask before ordering

Can you cross-reference a GH grade to ASTM or AMS?

Yes. GH4169 is the GB equivalent of Inconel 718 (N07718/AMS 5662); GH3030 sits close to Nimonic 75; GH3128 is a Ni-Cr-W-Mo alloy with no exact ASTM equivalent. We will put the comparison and the actual heat chemistry on the quotation so your design authority can approve it.

What is the maximum service temperature of Inconel 625 wire?

Continuous service is normally quoted at 980 °C for oxidation resistance and about 650 °C where creep strength governs. Above 650 °C under load, 718 or X-750 in the aged condition is usually the better answer.

Do you supply in the annealed or cold-drawn condition?

Both. Annealed for forming and welding, cold-drawn or spring temper where strength and straightness matter. Hardness, tensile and grain size can be specified on the order confirmation.

Is Monel 400 suitable for seawater?

Yes — Monel 400 resists flowing seawater and is widely used in marine hardware, but it is susceptible to crevice attack and to sulphur-bearing stagnation. Monel K500 adds strength; for severe chloride pitting, a C-type alloy is more conservative.

Ready to specify Nickel-Based Alloys?

Send the grade, size, quantity and service conditions. An engineer replies within 24 hours with a quotation and, if useful, a grade recommendation.

WhatsApp UsContact Us