Skip to content
Home / Products / Welding Metals / Ni-Cu Filler Wire
Ni-Cu Filler Wire

At a glance

Classification
ERNiCu-7 (Monel 60 type)
Composition
Ni65 / Cu28 / Ti
Diameter
0.8 – 3.2 mm
Form
TIG rod / MIG spool
Service
Seawater, HF, caustic
Certification
MTR + batch chemistry
Ni-Cu Filler Wire · ERNiCu-7

Nickel-Copper Filler Wire for Monel and Seawater Joints.

ERNiCu-7 in TIG rods and MIG spools, matched to Monel 400 and K500. Marine and chemical service where the weld has to corrode at the same rate as the parent metal — not faster.

  • ERNiCu-7 to AWS A5.14
  • 0.8 – 3.2 mm, rod or spool
  • Matches Monel 400 / K500
  • Titanium-stabilised deposit
One filler, one family

Monel welds with ERNiCu-7 — nothing else behaves the same.

Nickel-copper alloys depend on a continuous nickel-copper matrix for their seawater resistance. Substituting a nickel-chromium filler leaves a weld that is cathodic to the parent metal, and the parent corrodes preferentially at the toe of the weld.

ERNiCu-7 is titanium-stabilised to control porosity, which is the other common problem in Monel welding. We supply it with the deposit chemistry per batch and a reminder on the certificate: low heat input, clean joint, no preheat.

Where ERNiCu-7 is used

Four joint types that need this filler

The filler is fixed by the base metal family; the variables are heat input and cleanliness.

Monel 400

Matching base metal

Seawater and chemical service where the weld must match parent corrosion.

N04400
Monel K500

Age-hardened Monel

Welded in the annealed condition, then aged; ERNiCu-7 matches the matrix.

N05500
Dissimilar

Monel to steel

Nickel-copper to carbon steel transitions in marine systems.

ButteredMarine
Repair

Cast iron and Monel repair

Used for repair welds where a machinable, corrosion-resistant deposit is needed.

RepairMachinable
Sizes & forms

Rods, spools and cut lengths

TIG for root passes and repair, MIG for production and cladding.

TIG rod

1.6 – 3.2 mm

Root and repair

1 m lengths in sealed tubes; the surface stays clean until the arc starts.

  • Root passes
  • Repair welding
  • Manual TIG
MIG wire

0.8 – 1.2 mm

Production

Layer wound for consistent feeding on orbital and robotic equipment.

  • Production welding
  • Orbital
  • Cladding
Strip

to drawing

Automated TIG

Strip and preformed rings for tube-to-tubesheet and automated joints.

  • Tube-to-tubesheet
  • Automatic TIG
  • Rings

Welding Monel to steel and unsure about dilution? Send the joint detail — we advise on buttering and heat input.

Ask about dissimilar joints →
Classification & forms

ERNiCu-7 in the forms you weld with

One classification, three delivery forms, all from the same batch route.

01

Classification

ERNiCu-7

Monel 400 / K500 matching
AWS A5.14 · Ni65 / Cu28 / Ti

ERNiCu-7 (rod)

Manual TIG and repair
1.6 – 3.2 mm · 1 m

ERNiCu-7 (spool)

MIG and orbital
0.8 – 1.2 mm · 12.5 kg

Cross-reference

Monel 60 type
AWS / EN ISO 18274
02

Forms

TIG rod

Sealed tube, 1 m
1.6 – 3.2 mm

MIG spool

Layer wound
0.8 – 1.2 mm

Strip

For rings and automation
to drawing

Cut lengths

to drawing
on request

For K500 base metal, weld in the annealed condition and age afterwards — welding aged material risks cracking in the heat-affected zone. Send your specification — our engineers confirm availability and test values before you order.

Deposit properties

What the deposit has to match.

The deposit must match the parent metal in corrosion behaviour, not only in strength. Values below are typical for the as-welded deposit and are confirmed per batch.

Porosity is the main defect risk with nickel-copper fillers; the titanium addition and a clean, dry joint are both part of the control.

Tensile strength

As welded, typical

≈ 480 MPa

Yield strength

As welded, typical

≈ 240 MPa

Elongation

As welded

≥ 25%

Composition

Deposit, nominal

Ni65 / Cu28 / Ti

Interpass temp

Recommended maximum

≤ 150 °C

Preheat

Monel base metal

None
Packaging & handling

Dry, clean and sealed.

Nickel-copper filler is sensitive to moisture pickup, which shows up as porosity in the first pass.

Sealed tubes

Rods protected until opening.

TIG

Layer-wound spools

Stable feeding for orbital.

MIG

Batch chemistry

Deposit analysis per batch.

Documentation

Dry packing

Moisture barrier for sea freight.

Export

Cut lengths

to drawing for automation.

Automation

Neutral labels

For OEM supply.

OEM

Do not preheat Monel. Preheat increases dilution and porosity risk; clean the joint and control interpass temperature instead.

How an order runs

From your drawing to a labelled spool.

Five controlled steps, each with a named output — so nothing is agreed verbally and lost between shifts.

RFQ review

Drawing & requirement review

We check grade, size, temper, tolerance, packing and delivery date against what the drawing actually needs — and flag anything the process cannot hold.

Review focusRequirements confirmed
Grade

Grade and cross-reference

ERNiCu-7 confirmed against your existing grade number, with datasheet and typical test values issued before the order is placed.

Process outputGrade locked
Manufacturing

Wire drawing

Drawn and cleaned to a lubricant-free surface before packing.

Process focusDimensional control
Heat treatment

Cleaning and packing

Degreased, dried and sealed in tubes or layer-wound spools.

Process focusTemper & properties
Quality control

Inspection and dispatch

Chemistry, mechanical properties, dimensions and surface checked against the order, then packed for export with the documents inside the case.

Final outputMTR + COC issued
Industries & applications

Where nickel-copper joints are specified

Four service environments that need the Monel family end to end.

Marine: Seawater systems
Marine

Seawater systems

Piping, strainers and pump parts welded in Monel.

  • Seawater piping
  • Strainers
  • Pump casings
Chemical: Hydrofluoric and caustic
Chemical

Hydrofluoric and caustic

Service where nickel-copper is the specified alloy.

  • HF handling
  • Caustic plant
  • Reactor internals
Desalination: Brine and condenser parts
Desalination

Brine and condenser parts

Chloride resistance without pitting at the weld toe.

  • Condenser parts
  • Brine piping
  • Heat exchanger shells
Repair: Cast iron and Monel repair
Repair

Cast iron and Monel repair

Machinable, corrosion-resistant repair deposit.

  • Cast iron repair
  • Monel repair
  • Pump bodies
Why D GO TOP

The filler that keeps the parent metal intact.

A mismatched filler does not fail in the weld — it makes the parent metal corrode at the weld toe.

Classification

ERNiCu-7 to AWS A5.14

The correct nickel-copper filler, not a substitute.

Chemistry

Ti-stabilised deposit

Controlled porosity in the first pass.

Cleanliness

Degreased and sealed

Moisture pickup is the main porosity source.

Advice

No preheat, low interpass

Parameters that suit the alloy family.

Documentation

Batch deposit chemistry

For procedure qualification.

Volume

5 kg to 200 kg

Trial tubes and production spools.

ERNiCu-7AWS A5.14
Ni65 / Cu28Deposit
0.8 – 3.2 mmDiameter
SealedPackaging
Application cases

Three Monel joints and what they needed

Each had a corrosion or porosity problem that traced back to filler or heat input.

ERNiCu-7 for seawater strainer bodies
Marine · featured

ERNiCu-7 for seawater strainer bodies

Weld toe corrosion traced to a nickel-chromium filler used as a substitute; ERNiCu-7 restored the matching corrosion behaviour.

FillerERNiCu-7
Diameter2.4 mm
ProcessTIG
K500 pump parts, welded then aged
Chemical

K500 pump parts, welded then aged

Parts welded in the annealed condition with ERNiCu-7, then aged to hardness, with no heat-affected zone cracking.

FillerERNiCu-7
Diameter1.2 mm
ProcessMIG
Cast iron housing repair
Repair

Cast iron housing repair

Machinable nickel-copper deposit for a seawater pump housing, machined back to tolerance after welding.

FillerERNiCu-7
Diameter3.2 mm
ProcessTIG
Request a quotation

Send the joint. Get the right filler and parameters.

Tell us the base metals, thickness and service. We confirm the classification and quote rods or spools within 24 hours.

  • ERNiCu-7 with batch deposit chemistry
  • Advice on dissimilar joints and buttering
  • TIG rods and MIG spools from stock
Order questions

Ni-Cu filler FAQs

Questions about welding Monel and nickel-copper alloys.

Can I use ERNiCr-3 on Monel?

No. A nickel-chromium filler makes the weld cathodic to Monel and the parent metal corrodes at the weld toe. Use ERNiCu-7.

Should Monel be preheated?

No. Preheat increases dilution and porosity. Clean the joint and keep interpass below 150 °C.

How do I weld K500?

Weld in the annealed condition, then age. Welding aged K500 risks heat-affected zone cracking.

Why is the first pass porous?

Usually moisture or contamination. Keep rods sealed, clean to bright metal and use dry argon.

Do you supply 1 m rods?

Yes, 1 m lengths in sealed tubes, from 1.6 to 3.2 mm.

What is the minimum order?

One tube of rods or one 12.5 kg spool.

Related products

Other welding products

Keep reading

Guides and case studies

WhatsApp UsContact Us