Skip to content
Home / Products / Nickel-Based Alloys / Chinese GH Grades
Chinese GH Grades

At a glance

Grades
GH4169 · GH3030 · GH3128 · GH2132
Diameter
0.1 – 8.0 mm
Service temp
600 – 950 °C by grade
Condition
Annealed / solution + aged
Equivalent
718 · Nimonic 75 · A286 (GH3128: none)
Certification
MTR + COC
Chinese GH Grades · GH4169 · GH3030 · GH3128

Chinese GH Superalloy Wire, With the Western Equivalent Printed On It.

GH4169, GH3030, GH3128 and GH2132 drawn to 0.1 mm, with the ASTM or AMS equivalent stated on the certificate. For plants running Chinese specifications that still buy to international acceptance.

  • GH4169 · GH3030 · GH3128 · GH2132
  • 0.1 – 8.0 mm drawn wire
  • ASTM / AMS equivalent on the MTR
  • Chemistry to GB/T and plant specs
GH series, translated

The same alloy, a different numbering system.

GH4169 is Inconel 718. GH3030 is close to Nimonic 75. GH3128 is a nickel-chromium-tungsten alloy with no single Western equivalent, which is exactly why the chemistry has to be reported rather than replaced by a grade name.

Buyers outside China often receive GH wire without a cross-reference and cannot qualify it. We issue the GB/T chemistry alongside the nearest ASTM or AMS equivalent, so the document can be reviewed by both sides of the supply chain.

Cross-reference

Four GH grades and what they replace

Where an exact equivalent exists we say so; where it does not, we report the chemistry instead of guessing.

GH4169

≈ Inconel 718

Ni-Cr-Fe with Nb and Mo, age hardened for fasteners and turbine parts.

≈ N07718Aged
GH3030

≈ Nimonic 75

80/20 nickel-chromium for combustion chambers and low-stress hot parts.

≈ N06075800 °C
GH3128

Ni-Cr-W, no direct equivalent

Solid-solution strengthened for 950 °C service; chemistry reported in full.

Ni-Cr-W950 °C
GH2132

≈ A286

Iron-based with nickel and titanium, age hardened for fasteners.

≈ S66286
Drawing capability

Three ranges for GH grades

GH grades behave like their Western equivalents — the drawing route is set per grade, not per name.

Fine wire

0.1 – 1.0 mm

Mesh, seals and springs

Drawn with inter-pass annealing, then finished to the required condition.

  • Spring wire
  • Mesh
  • Seal wire
Standard wire

1.0 – 4.0 mm

Fasteners and fixtures

Straightened and cut for heading, or spooled for welding.

  • Fastener blanks
  • Furnace fixtures
  • Filler wire
Heavy wire

4.0 – 8.0 mm

Structural and welding stock

Annealed or solution treated, straightened for automatic welding.

  • Structural wire
  • Welding stock
  • Supports

Need a GH grade we have not listed? Send the GB/T number — we check the chemistry and the equivalent.

Send the GB/T number →
Grades & forms

GH grades with an international cross-reference

The cross-reference is issued with the certificate, not left to the buyer to research.

01

Grades

GH4169

≈ Inconel 718, age hardened
GB/T · Ni52 / Cr19 / Nb5

GH3030

≈ Nimonic 75, 800 °C
GB/T · Ni80 / Cr20

GH3128

Ni-Cr-W, 950 °C
GB/T · Ni balance / Cr20 / W8

GH2132

≈ A286, iron-based
GB/T · Fe / Ni25 / Cr15

Cross-reference

Send a grade for mapping
GB / ASTM / AMS
02

Forms

Round wire

Spooled, annealed
0.1 – 8.0 mm

Straightened lengths

For heading and machining
to 4 m

Coil

Continuous
5 – 200 kg

Flat wire

On request
0.2 – 3.0 mm thick

Where no exact equivalent exists, the full chemistry is reported rather than a misleading grade substitution. Send your specification — our engineers confirm availability and test values before you order.

Typical properties

Chemistry first, equivalent second.

Because several GH grades have no exact Western twin, the chemistry on the certificate is the primary evidence; the cross-reference is a convenience for reviewers.

Mechanical values depend on the heat treatment. GH4169 and GH2132 are supplied aged when strength is specified, and hardness is reported per lot.

GH4169 tensile

Solution + aged

≈ 1240 MPa

GH3030 service

Continuous, oxidising

≈ 800 °C

GH3128 service

Continuous, oxidising

≈ 950 °C

GH2132 tensile

Aged, typical

≈ 900 MPa

Elongation

Annealed grades

≥ 25%

Diameter tolerance

Cold drawn wire

h9 / drawing
Condition & packing

Delivered with the cross-reference attached.

The condition and the equivalent are both part of the document package.

Annealed

Soft for forming before ageing.

GH4169 / GH2132

Solution + aged

Full strength as delivered.

Aged

Bright annealed

Oxide-free for mesh and springs.

Surface

Pickled

Descaled after hot working.

Surface

Straightened lengths

For heading and thread rolling.

Forming

Spooled coil

Even tension for automated feed.

Packaging

The certificate carries both the GB/T designation and the nearest ASTM or AMS equivalent, plus the full chemistry where no exact match exists.

How an order runs

From your drawing to a labelled spool.

Five controlled steps, each with a named output — so nothing is agreed verbally and lost between shifts.

RFQ review

Drawing & requirement review

We check grade, size, temper, tolerance, packing and delivery date against what the drawing actually needs — and flag anything the process cannot hold.

Review focusRequirements confirmed
Grade

Grade and cross-reference

GH4169 / GH3030 confirmed against your existing grade number, with datasheet and typical test values issued before the order is placed.

Process outputGrade locked
Manufacturing

Cold drawing

Work-hardening grades drawn in short passes with inter-pass annealing.

Process focusDimensional control
Heat treatment

Solution and ageing

GH4169 and GH2132 are aged to the specified hardness window before despatch.

Process focusTemper & properties
Quality control

Inspection and dispatch

Chemistry, mechanical properties, dimensions and surface checked against the order, then packed for export with the documents inside the case.

Final outputMTR + COC issued
Industries & applications

Where GH grades are specified

Four sectors where the drawing calls a GB/T grade but acceptance is international.

Aerospace: Fasteners and hot-section parts
Aerospace

Fasteners and hot-section parts

GH4169 to the equivalent of 718 for bolts and brackets.

  • Fastener blanks
  • Bracket wire
  • Lockwire
Furnace: Combustion and radiant parts
Furnace

Combustion and radiant parts

GH3030 for chambers and low-stress hot components.

  • Chamber wire
  • Radiant parts
  • Supports
Energy: Boiler and turbine internals
Energy

Boiler and turbine internals

GH3128 for 950 °C service where 800 series is not enough.

  • Turbine seals
  • Boiler supports
  • Expansion parts
Industrial: Replacement parts for imported equipment
Industrial

Replacement parts for imported equipment

Cross-referenced wire for plants maintaining Western-designed equipment.

  • Spare parts
  • Repair wire
  • Refurbishment
Why D GO TOP

Two numbering systems, one certificate.

The point of buying GH wire outside China is documentation, not the alloy itself.

Cross-reference

ASTM / AMS equivalent

Printed on the MTR next to the GB/T grade.

Chemistry

Full analysis

Reported where no exact equivalent exists.

Drawing

Short-pass schedules

GH grades drawn without edge cracking.

Heat treatment

Solution and ageing

Ageing to the specified hardness window.

Testing

Hardness and tensile

Values for the condition actually supplied.

Documentation

MTR + COC

One file acceptable to both buyer and end user.

4 gradesGH series
950 °CGH3128 service
GB / ASTMCross-referenced
AgedOn request
Application cases

Three GH orders, three documentation requirements

In each case the alloy was easy; the acceptance paperwork was the actual work.

GH4169 wire with 718 cross-reference
Aerospace · featured

GH4169 wire with 718 cross-reference

An MRO needed GH4169 recognised as 718 by a European auditor, with hardness values for the aged condition on the same certificate.

GradeGH4169
Diameter5.0 mm
ConditionAged
GH3030 chamber wire
Furnace

GH3030 chamber wire

Replacement wire for an imported furnace, matched by chemistry because the original grade designation was not available.

GradeGH3030
Diameter3.2 mm
ConditionAnnealed
GH3128 for 950 °C supports
Energy

GH3128 for 950 °C supports

Supplied with full chemistry and a statement that no exact AMS equivalent exists, so the designer could approve it on data rather than name.

GradeGH3128
Diameter4.0 mm
ConditionSolution
Request a quotation

Send the GB/T number. Get a cross-referenced quote.

Tell us the grade, condition, diameter and quantity. We confirm the chemistry and the nearest international equivalent, and quote within 24 hours.

  • GB/T grade plus ASTM / AMS equivalent
  • Full chemistry where no equivalent exists
  • Aged condition with hardness values
Order questions

GH grade FAQs

What buyers ask when GH wire has to pass an international review.

Is GH4169 the same as Inconel 718?

Compositionally yes, and it is normally accepted as an equivalent. The certificate states both designations so an auditor does not have to research it.

Which GH grade has no Western equivalent?

GH3128 is a nickel-chromium-tungsten alloy with no single AMS equivalent; we report the full chemistry instead of claiming a match.

Can you supply aged material?

Yes for GH4169 and GH2132, with hardness tested per lot and reported against the target.

Do you test to GB/T or ASTM?

Both, depending on the order. Tell us which standard the acceptance is written against.

What is the minimum order?

From 5 kg for standard grades; aged material usually from 20 kg.

What is the lead time?

2–3 weeks for annealed stock; 4–6 weeks for aged or non-standard diameters.

Related products

Other alloy wire families

Keep reading

Guides and case studies

WhatsApp UsContact Us