Welding Metals — Filler Wire from the Source Factory

Filler metals that match the parent metal, not just the name on the box — nickel-based, nickel-copper and stainless wires to AWS A5.14 and A5.9, in spools, coils and cut lengths, plus the process parameters to go with them.

4product series
0.8–3.2 mmfiller diameter
AWS A5.14classification
24 hWPS review

Products in this category

Four filler-metal series, each a separate page with grades, tolerances, forms and packing. Welding Process Support is an engineering service shipped with the filler, not a fifth series.

Grades and typical applications

Indicative data — the order confirmation carries the binding specification.

GradeUNS / GBKey dataTypical use
ERNi-1N0206199% Ni, Ti-stabilisedWelding commercially pure nickel, Ni200/Ni201
ERNiCr-3N06082Inconel 82 typeInconel 600/601, dissimilar Ni-alloy to steel
ERNiCrMo-3N06625Inconel 625 typeInconel 625, 718 repairs, 9% Ni steel, overlay
ERNiCrMo-4N10276Hastelloy C-276 typeC-276 matching; C-22 repairs (C-276-type deposit)
ERNiCu-7N04019Monel 60 typeMonel 400/K500, Ni-Cu to steel
ER308LS3088319Cr-10Ni, low C304/304L stainless
ER316LS3168317Cr-12Ni-2.5Mo, low C316/316L, mild chloride service
ER2209S3920922Cr-9Ni-3Mo-N duplexDuplex 2205, dissimilar duplex joints

How to choose

Three questions that decide the grade before price is discussed.

Match the filler to the service, not only to the parent metal.

Undermatching strength but overmatching corrosion resistance is normal practice for nickel alloys: ERNiCrMo-3 on Inconel 625 gives a weld as corrosion-resistant as the parent, which matters more than matching tensile strength.

Watch dilution on dissimilar joints.

Welding nickel alloy to carbon steel dilutes iron into the weld. Limit dilution to about one third, or use a buttering layer. ERNiCr-3 tolerates dilution better than ERNiCrMo-3 in most cases, and we will review the joint design with you.

Duplex needs heat input control.

ER2209 wants 0.5–2.5 kJ/mm and an interpass temperature below 150 °C to keep the ferrite/austenite balance. Too much heat gives brittle intermetallics; too little gives inadequate ferrite.

Quality documents with every lot

01

Heat traceability

Coil and spool numbers linked to the melt.

02

EN 10204 3.1

Chemistry, mechanicals, dimensions.

03

Certificate of conformity

Against the agreed standard.

04

Third-party inspection

SGS, BV or TÜV on request.

Questions buyers ask before ordering

Which filler for Inconel 625 to carbon steel?

ERNiCrMo-3 (Inconel 625 type) is the usual answer, with a nickel-based buttering layer on the steel side if dilution is a concern. ERNiCr-3 is a lower-cost alternative where corrosion demand is moderate.

Do you supply spools to EN ISO 14343 / AWS A5.14?

Yes. Spools are supplied to AWS A5.14 for nickel alloys and A5.9 for stainless, with the classification, heat number and lot traceability on the label and in the MTR.

Can you review our WPS?

Send the drawing, parent metals, thickness and process and we will return a parameter review within 24 hours — current, voltage, travel speed, gas and interpass limits. It is a review, not a certified WPS; formal qualification remains with your welding engineer.

What is the minimum order for cut-length filler?

Cut lengths are normally quoted from 5 kg per diameter in 1,000 mm lengths; spools from 5 kg (0.8–1.2 mm). Pre-formed rings are quoted individually once we have the joint drawing.

Ready to specify Welding Metals?

Send the grade, size, quantity and service conditions. An engineer replies within 24 hours with a quotation and, if useful, a grade recommendation.

WhatsApp UsContact Us