Low gas content, no drawing residue and a thickness tolerance that lets a spot-weld schedule repeat — the three things vacuum and cell assembly actually need.
The three requirements that decide whether the wire works here.
Drawing residue and handling oil are the main source of outgassing and weld porosity — so the wire is ultrasonically degreased, dry-packed and shipped with a cleaning certificate.
A tab weld schedule only repeats if thickness and burr stay inside a narrow window, coil after coil. Burrs also puncture separator film downstream.
Heat number on the spool label, MTR and cleaning record together, so a finished cell lot can be traced back to one melt of nickel.
Starting points — the final choice follows the atmosphere, cycle and geometry.
| Application | Grade | Typical size | Why |
|---|---|---|---|
| Battery tab | Ni200 strip | 0.10–0.30 mm, ±0.005 | Ultrasonic or spot welded to Al/Cu |
| Cell connector | Ni201 strip | 0.15–0.50 mm | Better where heat is applied |
| Vacuum feedthrough | Ni200 wire | 0.20–2.0 mm | Low outgassing after cleaning |
| Electrode / anode | Ni200 bar | per drawing | Plating and electrolysis |
| Evaporation filament | 99.9% Ni wire | 0.5–1.5 mm | Low trace elements |
Bright annealed wire is ultrasonically degreased and packed dry; we can supply a cleaning certificate. Actual outgassing depends on your vacuum bake-out, so we quote surface cleanliness rather than a chamber number.
Thickness tolerance ±0.005 mm and camber under 1 mm per metre on tab strip. Edge quality is slit, burr-controlled, because burrs puncture separator film.
Yes, traverse wound on plastic spools or in level-wound coils up to 200 kg, with interleaving paper on request for scratch-sensitive surfaces.
Service temperature, atmosphere, cycle time and joint design — with those four numbers we can recommend a grade and size with the life you need.