Element design starts from two numbers you already know — supply voltage and target wattage — and ends with a wire diameter and length. Four arithmetic steps get there; most errors come from skipping the second and third. Send us your numbers and our factory engineers will verify them before you cut the wire.

Resistance from wattage

For a single-phase element: R = V² / P. A 230 V, 2,000 W element needs 26.5 Ω total. That number, divided by the resistivity of the grade, gives the wire length.

Length from resistivity

Resistance per metre is R′ = ρ / A, where ρ is resistivity and A the wire cross-section. For Ni80Cr20 (ρ = 1.09 µΩ·m), a 1.0 mm wire (A = 0.785 mm²) gives about 1.39 Ω/m. The 2,000 W element therefore needs 26.5 / 1.39 ≈ 19 m of 1.0 mm wire.

Check the surface load

Divide wattage by the wire surface area: q = P / (π · d · L). For the example above, 2,000 W over 19 m of 1.0 mm wire is about 3.3 W/cm² — comfortable in free air for Ni80Cr20. Wound into a ceramic groove or coiled tightly, the effective load rises and the allowable value drops; your element geometry, not the alloy, sets the real limit.

EnvironmentTypical allowable surface load (Ni80Cr20)
Free air, straight or widely spaced4–8 W/cm²
Coiled on ceramic supports2–4 W/cm²
Embedded in metal sheath8–15 W/cm² (conduction cooled)
Embedded in insulation (mica, MgO)2–6 W/cm²

Where calculations meet reality

  • Resistivity has a tolerance. We hold ±3% on request; a ±5% resistivity band is a ±5% wattage band on a fixed-voltage element.
  • Hot resistance differs from cold. An element sized on cold resistance runs below target wattage until it is hot. FeCrAl is flatter than nichrome — a Kanthal A-1 type wire reaches about 1.04× its 20 °C value at 1,000 °C, Ni80Cr20 about 1.09×. Size on hot resistance.
  • Tolerance stacks. Diameter tolerance P5 on 1.0 mm is ±0.02 mm — about ±4% on resistance by itself. Specify resistance per metre instead of diameter alone when wattage matters.

Send us the three numbers

Voltage, wattage and element geometry (length available, winding form). We will return a sized option for both nichrome and FeCrAl with the resistance per metre we can certify — usually the fastest way to a drawing that survives production.

Key takeaways

  • Two formulas cover most element sizing. R = V²/P gives resistance from supply and power; L = R·A/ρ gives length from resistivity and cross-section.
  • Check surface load after the arithmetic. A geometry that satisfies the resistance target can still be thermally impossible.
  • Resistivity is temperature-dependent. Use the value at working temperature, not the 20 °C figure, or the cold-start current will be wrong.
  • Verify the result against a known element. Comparing a calculated design to an existing element of known life catches most sizing errors before a build.

Frequently asked questions

What is the basic formula for heating element resistance?

Resistance equals supply voltage squared divided by required power: R = V² / P. For a 230 V supply and 2,000 W the target resistance is about 26.5 Ω at operating temperature.

How do I get wire length from resistance?

Length equals resistance multiplied by cross-sectional area, divided by resistivity: L = R · A / ρ. Area for round wire is π·d²/4. Keep units consistent — resistivity in Ω·m, diameter and length in metres.

Why is my calculated wattage wrong when I measure it?

The usual causes are using 20 °C resistivity instead of the value at working temperature, an element that is not at thermal equilibrium when measured, and supply voltage that differs from nominal. Measure hot, and measure the actual supply.

What is surface load and why does it matter?

Surface load is the power dissipated per unit of wire surface area, usually in W/cm². It sets how hot the wire runs relative to the element. Exceed the alloy and atmosphere limit and the element overheats even though the resistance calculation was correct.

Can I use the same calculation for flat and stranded wire?

Yes, with the right cross-section. Flat wire uses width × thickness; stranded constructions need the effective metallic area, not the overall diameter, since the outer envelope includes voids.

D GO TOP Technical Team

Process Engineering · Wire Drawing & Heat Treatment

Our engineers support grade selection, element sizing and tolerance review for nickel, nickel-chromium, FeCrAl and superalloy wire. More about our technical team.

Next step

Send three numbers, get an answer

Diameter or cross-section, working temperature, and required power or resistance. We reply within 24 hours with the grade that fits, and with where the margin sits.

WhatsApp UsContact Us