A cell assembler in Eastern Europe was seeing intermittent weld failures traced to strip thickness variation. We supplied 0.15 mm Ni200 strip at ±0.005 mm with controlled burr — and the weld schedule finally repeated.

GRADE:  Ni200 (N02200)SIZE:  0.15 × 40 mm stripTOLERANCE:  ±0.005 mmPACKING:  Traverse wound

The problem

Ultrasonic tab welding was producing occasional weak joints. The weld energy had been tuned to a nominal 0.15 mm strip; incoming material varied enough across suppliers that some lots welded cold. Scrap and rework were concentrated on a single production line.

The diagnosis

Measurement of incoming coils showed thickness spread of up to 0.02 mm within a single coil — a 13% variation on 0.15 mm. No ultrasonic schedule can repeat through that. The strip also carried light drawing lubricant on one side, which varied the weld interface.

What we supplied

  • Ni200 strip at 0.15 × 40 mm, thickness held to ±0.005 mm across the coil.
  • Slit edges with a controlled burr height, because burrs were puncturing separator film downstream.
  • Ultrasonic degrease plus a cleaning certificate per lot.
  • Traverse-wound 50 kg coils with paper interleaving.

The result

Weld strength variation tightened to the point where the customer froze the weld schedule across three shifts. Thickness Cpk on incoming strip is now reported per lot, and the line consumes strip from a single qualified source.

Application example, anonymised from our order book. Tab thickness, width and edge condition are quoted to your weld schedule.

Other application examples

Same problem, different alloy?

Send the application data — atmosphere, temperature, cycle and current specification. We will tell you what we would change and quote both options.

WhatsApp UsContact Us